Surgical and diagnostic silicone parts fail quietly. A seal that tears on the fortieth instrument insertion, a lens that hazes under the slit lamp, a pipette tip that sheds a particle into a sample – none of these show up in a first-article inspection.
We mould components for the sterile field, the eye and the laboratory: wound protectors, trocar seals, intraocular lenses, endoscope accessories and diagnostic parts where the specification is written in tolerances and extractables rather than in appearance.
Parts that enter the sterile field or the body, and the tooling discipline that goes with them.
Patient-side sensors, sample-contact parts and lab consumables where cleanliness is the product.
Silicone is soft enough to be forgiving, which also means a poorly finished parting line can shed material every time an instrument passes through a seal. We finish and inspect contact edges rather than relying on the mould alone, and we quantify particulates on the production part for wound protectors and trocar seals instead of quoting a cleanroom class.
The seal is compressed and wiped hundreds of times in a single procedure. Tear initiation at the aperture is the usual failure path, and it starts at a moulded edge that looked acceptable on the bench. We specify tear strength against the radial expansion of the actual instrument diameter, and validate with insertion cycles on production parts.
Silicone that is transparent in a 2 mm plaque can still haze in a 0.6 mm lens body, because light path length, cure completeness and surface finish all interact. For intraocular lenses and transparent covers we control refractive index, transmission and haze on the finished geometry, and we treat cure time as a specification item rather than a machine setting.
In a diagnostic consumable the part is in contact with the sample or the reagent. Volatile siloxanes and unreacted low-molecular-weight species migrate into the fluid, and the effect appears as drift, false elevation or a failed validation run. Post-cure and extraction profiles are chosen for the contact medium, not for a generic medical grade.
Pipette tips, piston seals and cryotube seals are specified at tolerances where tool wear over 100,000 shots matters as much as the first shot. We build in cavity-level dimensional tracking so a drift is caught on the tool before it becomes a rejected lot.
Typical envelope for surgical, ophthalmic and diagnostic parts – confirm against your device specification.
| Property | Typical range | What it controls |
|---|---|---|
| Hardness | 30-70 Shore A (seals 40-60 A, optical parts 50-70 A) | Sealing force, instrument feel, dimensional stability of thin optical sections |
| Optical performance | Transmission and haze specified on the finished part | Usable vision through an IOL or cover; cosmetic defects that are not cosmetic |
| Tear strength | ≥ 25 kN/m on standard test pieces | Survival of trocar seals and wound protector rings through repeated use |
| Dimensional tolerance | Typically ±0.05 mm on critical features, tighter on request | Assembly with rigid housings, instrument fit, sample volume reproducibility |
| Post-cure / extraction | Volatile and extractable profile matched to contact medium | Drift and interference in diagnostic and ophthalmic applications |
Moulding runs under ISO 13485 in an ISO Class 8 cleanroom, with lot traceability from compound batch to shipped carton. For implantable and ophthalmic programmes we hold the process records that a notified body asks for during a technical file review, including cure verification and environmental monitoring data.
Biocompatibility testing (ISO 10993) is carried out on the production compound and, where the geometry changes the exposed surface area materially, on the finished part. Extractables and leachables work is scoped to the contact medium – saline, reagent, ophthalmic viscosurgical device – rather than run as a generic panel.
We work through the drawing, the contact medium, the sterilisation route and the acceptance tests before quoting, because a tolerance that cannot be measured in production is not a specification.
Compound and cure profile chosen against extractables and optical requirements, not only hardness.
Cavity-level dimensional report, plus functional testing on the failure mode that matters for the part.
In-process checks, cavity traceability and documented change control before any process change reaches your supply.
We mould silicone lens bodies with haptics, including the optical surface. Whether the programme is viable depends on the dioptric range and the inspection method you require – send the drawing and we will tell you what we can hold.
We test the finished part rather than quoting a cleanroom class, because the class describes the room and not the part. The result depends on geometry and finishing, so it is established during validation and then controlled in production.
Yes, scoped to the contact medium. A generic panel rarely answers the question a diagnostic manufacturer is actually asking, so we agree the medium and the detection limits first.
Each cavity is measured separately and tracked over the tool life, so drift is visible per cavity instead of being averaged out in a lot report.
For many geometries yes – moulding in ISO Class 8 with controlled handling removes the need for a post-mould wash that would itself introduce residue.
Typically 8-12 weeks from design freeze to validated production for a new tool, of which tooling is about half. Validation scope drives the rest.
Particulate counts, insertion cycles, haze limits, extractable thresholds – tell us which one your validation stands or falls on. That is the number we design the tool around.