How to Select Silicone Hardness for Medical Components

10/29/20260

Durometer is one of the first numbers on a medical silicone drawing and one of the easiest to get wrong. It is usually copied from an existing part, or picked because “it felt right”, and then never revisited — until the seal leaks, the cushion is uncomfortable, or the part will not demould. This guide explains what hardness actually controls and how to choose it.

What Durometer Measures

Hardness is the resistance of the material to indentation. For silicone it is normally reported on the Shore A scale, measured according to ISO 7619-1 or ASTM D2240. Softer materials below about 20 Shore A are sometimes reported on the Shore 00 scale, and very hard compounds move to Shore D. Small or thin specimens may be better measured by IRHD (ISO 48), because a durometer foot needs enough material under it to give a repeatable reading.

What Hardness Actually Controls

  • Seal force. Softer compounds conform to mating surfaces and seal at lower compression; harder compounds need more deflection to seal but resist extrusion.
  • Conformability and comfort. Skin-contact parts need softness, but softness unsupported by geometry causes tackiness and demoulding problems.
  • Insertion and actuation force. Septa, valves and stoppers must reseal after puncture — too soft and they core, too hard and the insertion force rises.
  • Wear and tear resistance. Softer grades generally tear more easily; high-tear compounds exist but are specified as a property, not inferred from durometer.
  • Processing behaviour. Softer grades tend to shrink more, flash more and stick to tooling.

Typical Ranges by Application

Application Typical range (Shore A) Why
Respiratory mask cushions, nasal pillows 30–50 Facial conformability and comfort
Static seals, gaskets, O-rings 40–60 Seal at low compression without extruding
Septa and resealing stoppers 50–70 Reseal after puncture, resist coring
Grips, overmolds, handles 50–70 Tactile feel with structural integrity
Keypads and button covers 40–60 Tactile response and return
Structural or snap-fit features 60–80 Hold shape, strip off the tool

These are starting points, not specifications. The right answer depends on wall thickness, the mating part and the load — which is why sampling two durometers is usually cheaper than guessing once.

Hardness Does Not Act Alone

A 60 Shore A part with a 0.8 mm wall feels softer than a 40 Shore A part with a 3 mm wall. Geometry moves perceived softness at least as much as durometer does, so specify hardness together with wall thickness, and review both at prototyping stage.

How to Specify It

  • Give a target and a tolerance — ±5 Shore A is the normal commercial band.
  • State the standard (ISO 7619-1 or ASTM D2240) and the scale (Shore A).
  • State when it is measured — after post-cure, conditioned at 23 ± 2 °C. Readings taken hot or straight out of the mould are not comparable.
  • If the feature is small or thin, agree the measurement method in advance, or specify IRHD.

FAQ

Does a softer durometer seal better?

Up to a point. Softer material conforms with less compression, but it also extrudes, creeps and tears more easily. Seal design and groove fill usually matter more than hardness alone.

Can I just copy the durometer from an existing part?

Only if the geometry and the mating part are the same. A durometer that works at one wall thickness can be wrong at another, and a different compound from a different supplier at “60 Shore A” is not necessarily the same material.

Why did hardness readings differ between our lab and the supplier?

Most often because of specimen thickness, measurement timing after post-cure, or temperature. Fix the standard, the specimen and the conditioning, and the numbers converge.

LSR Injection Molding · Compression Molding

Talk to the engineering team

Send a drawing or a project brief and get a manufacturability review, a process recommendation and a quotation.

Discuss your project with our engineering team


Leave a Reply

Your email address will not be published. Required fields are marked *